Share
Reflection Electron Microscopy and Spectroscopy for Surface Analysis
Zhong Lin Wang; Wang Zhong Lin (Author)
·
Cambridge University Press
· Paperback
Reflection Electron Microscopy and Spectroscopy for Surface Analysis - Zhong Lin Wang; Wang Zhong Lin
Choose the list to add your product or create one New List
✓ Product added successfully to the Wishlist.
Go to My Wishlists
Origin: U.S.A.
(Import costs included in the price)
It will be shipped from our warehouse between
Thursday, July 04 and
Tuesday, July 16.
You will receive it anywhere in United Kingdom between 1 and 3 business days after shipment.
Synopsis "Reflection Electron Microscopy and Spectroscopy for Surface Analysis"
This book is a comprehensive review of the theories, techniques and applications of reflection electron microscopy (REM), reflection high-energy electron diffraction (RHEED) and reflection electron energy-loss spectroscopy (REELS). The book is divided into three parts: diffraction, imaging and spectroscopy. The text is written to combine basic techniques with special applications, theories with experiments, and the basic physics with materials science, so that a full picture of RHEED and REM emerges. An entirely self-contained study, the book contains much invaluable reference material, including FORTRAN source codes for calculating crystal structures data and electron energy-loss spectra in different scattering geometries. This and many other features makes the book an important and timely addition to the materials science literature for researchers and graduate students in physics and materials science.
- 0% (0)
- 0% (0)
- 0% (0)
- 0% (0)
- 0% (0)
All books in our catalog are Original.
The book is written in English.
The binding of this edition is Paperback.
✓ Producto agregado correctamente al carro, Ir a Pagar.